. Prepare substrate, install grounding foil (
see full instructions for details). Prepare the ElectraGuard carefully: Catalyzed ElectraGuard should be used within six hours of mixing, therefore prepare only the quantity necessary for immediate use.
Add the pre-measured catalyst to epoxy base. Stir gently until the catalyst has been thoroughly mixed in (a low RPM drill may be used with a rotary mixing attachment but try to not beat air into the material). Allow the catalyzed mixture to stand 5 minutes.
Utilizing a short nap roller or brush, carefully apply a thin uniform coat of catalyzed ElectraGuard around perimeter walls, doorways etc (about 6" width and try to not get any on walls ;) After perimeter of room is completed utilize short nap rollers (18" wide with long handle extensions work best) to roll a thin uniform coat through out the remainder of the area. The initial coat will cover approximately 250 to 500 ft 2 per gallon.
Allow the initial coat to dry for 5-7 hours or longer and apply a second coat. Second coat coverage is approximately 500-600 ft2 per gallon. Allow the second coat to dry for 8 to 12 hours and apply a third cost. Third coat coverage is approximately 500-600 SF per gallon.
Finished floors may be opened to light traffic, under normal curing conditions, after 12 hours.
See full scale installation instructions for further details. Allow coats to cure for a minimum of 48 hours (good environmental airflow) or 72 hours (compromised environmental airflow) prior to proceeding to step 2 (topical coatings of Electrathane Sealer).
Thoroughly remove loose dirt and dust
cured ElectraGuard via sweeping (do not
use sweeping compounds). Remove
imperfections if any (such as bubbles
and splatters) from ElectraGuard via
light scraping followed by vacuuming.
Agitate ElectraThane sealant in
container prior to use, pour into clean
contaminant free bucket and mop on one
thin even coat using non linting
synthetic finish mops. Allow coat to dry
(depending on humidity and temperature)
for 60 to 90 minutes before
re-application of second thin coat. Two
coats are or more are recommended.
ElectraThane does not readily lend
itself to high speed polishing but has a
good as applied luster and excellent
slip resistance. Allow coats to cure for
a minimum of 12 hours prior to
proceeding to step 3 (topical coatings
of ElectraGlaze Floor Finish).
See full scale installation instructions
for further details.
Using a clean Rayon finish mop or wax
applicator, apply a minimum of one thin
even coat of ElectraGlaze allowing
finish to dry 2 to 4 hours prior to
allowing traffic on floor. Two coats are
recommended for optimum performance.
Buffing is not required unless high
mirror like shine is desired. Note:
Avoid application during high humidity
conditions, use thin coats ONLY.
See full scale installation instructions
for further details. The
ElectraGuard Tri-Layer ESD Flooring
System meets latest standard of
S2020-2007 for esd conductive flooring
and ANSI/ESD STM97.1-2006 resistance to
ground in combination with Operator /
Heel Grounders / ESD Flooring.
ElectraGuard Tri-Layer meets or exceeds
the requirements of Federal
Specifications LF-475a and SST-312b for
dimensional stability, resistance to
reagents and residual indentation.